Research on optical fiber current transducer using nv center in diamond

MetadataDetails
Publication Date2024-02-01
JournalJournal of Physics Conference Series
AuthorsQiang Song, Yang Lu, Dingqu Zhang, Sanlei Dang, Likun Xing
InstitutionsChina Electric Power Research Institute, China Southern Power Grid (China)

Abstract Diamond nitrogen-vacancy (NV) center has been widely employed in experimental magnetic field measurement using continuous wave optical detection magnetic resonance (ODMR), which makes it possible for current sensing. An optical fiber current transducer prototype using an NV center is built for electric power application. The DC measurement with an error of less than 4% within 500 A is realized, in which the error of 50 A to 450 A is better than 2%, and the low-frequency AC measurement is preliminarily realized. In this essay, the accuracy of low current measurement is primarily affected by system noise, while the accuracy of heavy current is mainly affected by the width of the ODMR resonance peak. Optimizing the optical path as well as sensing structure meanwhile updating the demodulation algorithm of the measured data is the following work to improve the measurement accuracy.

  1. 2020 - Challenge and Application Prospect of Power Intelligent Sensor Technology [J]
  2. 2021 - Panoramic Information Perception and Intelligent Grid [J]
  3. 2014 - Nitrogen-Vacancy Centers in Diamond: Nanoscale Sensors for Physics and Biology [J] [Crossref]
  4. 2015 - Magnetometry with nitrogen-vacancy defects in diamond [J]
  5. 2018 - Probing condensed matter physics with magnetometry based on nitrogen-vacancy centers in diamond [J] [Crossref]
  6. 2013 - Nanometre-scale thermometry in a living cell [J] [Crossref]
  7. 2019 - Principles and Techniques of the Quantum Diamond Microscope [J] [Crossref]
  8. 2010 - Optical properties of the nitrogen-vacancy singlet levels in diamond [J] [Crossref]
  9. 2019 - Identifying and mitigating charge instabilities in shallow diamond nitrogen-vacancy centers [J] [Crossref]