Fabrication and characterization of diamond nitrogen-vacancy center through argon ions etching

MetadataDetails
Publication Date2024-05-01
JournalJournal of Physics Conference Series
AuthorsXiaokui Zang, Zhiqiang Cao, Jing Liu, Guanghua Tong, Han Wang

Abstract The diamond nitrogen-vacancy center with a negative charge (NV − ) exhibits exceptional optical properties and enables highly sensitive detection of multiple physical quantities. The development of a simple and efficient method for fabricating NV − centers in diamonds holds significant importance in promoting their widespread application. The fabrication method of NV − centers is explored in this work, utilizing high-energy photons emitted by argon ions to induce vacancies in type Ia diamond substrates. The processed samples are optical characterized, and the characteristic peak and zero phonon line corresponding to the NV − center can be observed in Raman and photoluminescence spectra respectively. The concentration of NV − centers in samples could reach up to 153.9 ppb, estimated by integrating the fluorescence intensity of the photoemission spectrum. The samples exhibit the spin characterization of NV − centers, which achieve a maximum contrast of 1.5% in the optical detection magnetic resonance (ODMR) spectra.

  1. 2014 - Nitrogen-Vacancy Centers in Diamond: Nanoscale Sensors for Physics and Biology[J] [Crossref]
  2. 2019 - Principles and Techniques of the Quantum Diamond Microscope[J] [Crossref]
  3. 2008 - High-sensitivity diamond magnetometer with nanoscale resolution[J] [Crossref]
  4. 2017 - Solution nuclear magnetic resonance spectroscopy on a nanostructured diamond chip[J] [Crossref]
  5. 2016 - High-density NV sensing surface created via He+ ion implantation of 12C diamond[J] [Crossref]
  6. 2012 - Nitrogen-Vacancy-Assisted Magnetometry of Paramagnetic Centers in an Individual Diamond Nanocrystal[J] [Crossref]
  7. 2005 - Reduction of plasma-induced damage in SiO2 films during pulse-time-modulated plasma irradiation[J] [Crossref]
  8. 2006 - Effects of Thermal Annealing for Restoration of UV Irradiation Damage during Plasma Etching Processes[J] [Crossref]
  9. 2017 - Vacuum ultraviolet radiation emitted by microwave-driven argon plasmas[J] [Crossref]