Skip to content

Monte Carlo Explicitly Correlated Second-Order Many-Body Green’s Function Calculations of Semiconductor Band Gaps

MetadataDetails
Publication Date2024-09-28
JournalThe Journal of Physical Chemistry C
AuthorsJulio César Cruz, So Hirata
InstitutionsUniversity of Illinois Urbana-Champaign
Citations1

A systematically converging series of ab initio, post-density-functional, size-consistent, electron-correlated approximations is desired for predictive computing o felectronic band structures of insulating, semiconducting, and metallic solids. A series that meets all of these desiderata (except the applicability to metals) is ab initio many-body Green’s function theory based on Gaussian-type-orbital (GTO) basis sets. Here, its leading-order approximation, the second-order Green’s function (GF2) method in the diagonal and frequency-independent approximations with the aug-cc-pVDZ basis set, is applied to the fundamental band gaps of three semiconductors (diamond, silicon, and silicon carbide in the zincblende structure) using cluster models. Corrections are made to the basis-set-incompleteness errors by the explicit-correlation (F12) ansatz (GF2-F12) for the valence band edges. The crystals are modeled as surface-passivated clusters of increasing sizes, whose wave functions are expanded by up to 2709 GTO basis functions. Immense computational costs of these calculations are overcome by the highly scalable stochastic algorithm of the Monte Carlo GF2-F12 method, whose operation cost per state increases only as a cubic power of system size, which has a tiny memory footprint and easily achieves near-perfect parallel efficiency on thousands of CPUs or on hundreds of GPUs. The correlated, F12-corrected highest-occupied and lowest-unoccupied molecular-orbital energy (HOMO-LUMO) gap is 5.78 ± 0.07 eV for C<sub>87</sub>H<sub>76</sub> as compared with the experimental value of the fundamental (indirect) band gap of bulk diamond at 5.48 eV. The correlated, F12-corrected HOMO-LUMO gaps for Si<sub>75</sub>H<sub>76</sub> and Si<sub>32</sub>C<sub>43</sub>H<sub>76</sub> are 2.56 ± 0.15 eV and 3.50 ± 0.12 eV, respectively, which are expected to decrease further with increasing cluster sizes. As a result, the experimental fundamental (indirect) band gaps of bulk silicon and silicon carbide are 1.17 eV and 2.42 eV, respectively.