Salt-coated air oxidation nanodiamond surface purification with a photoluminescence spectroscopy quality control
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-09-18 |
| Journal | Nanotechnology |
| Authors | Š”. Š. Давинов, T. Yu. Kolomiets, Dongxue Bi, V. V. Sychev |
| Institutions | Baikov Institute of Metallurgy and Materials Science, P.N. Lebedev Physical Institute of the Russian Academy of Sciences |
Abstract
Section titled āAbstractāAbstract Emerging fields of quantum technologies and biomedical applications demand pure nanodiamonds (NDs) with well-defined surface chemistry. Therefore, an inexpensive, scalable and eco-friendly ND surface purification technology is required. In this study, we report our method, salt-coated air oxidation (SCAO) thermal annealing, to achieve uniform purification of a ND surface without the loss of diamond material. A photoluminescence (PL) spectroscopy quality control method is proposed to evaluate the degree of purification. The presence of an isoemission point in the set of nitrogen vacancy (NV) center PL spectra, obtained through the photochromic effect, is examined as a surface purity indicator. The ratio of the NV centers in NDs after the SCAO treatment was determined by decomposing the PL spectra using the non-negative matrix factorization technique.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2013 - The nitrogen-vacancy colour centre in diamond [Crossref]
- 2014 - Electronic structure of the silicon vacancy color center in diamond [Crossref]
- 2010 - Fabrication of single optical centres in diamondāa review [Crossref]
- 1976 - Optical studies of the 1.945 eV vibronic band in diamond [Crossref]
- 2010 - Spin-polarization mechanisms of the nitrogen-vacancy center in diamond [Crossref]
- 2000 - Stable solid-state source of single photons [Crossref]
- 2003 - Long coherence times at 300 K for nitrogen-vacancy center spins in diamond grown by chemical vapor deposition [Crossref]
- 2013 - Diamond NV centers for quantum computing and quantum networks [Crossref]
- 2016 - Diamond quantum devices in biology [Crossref]