Creation, stabilization, and investigation at ambient pressure of pressure-induced superconductivity in Bi 0.5 Sb 1.5 Te 3
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2025-02-04 |
| Journal | Proceedings of the National Academy of Sciences |
| Authors | Liangzi Deng, Busheng Wang, Clayton Halbert, Daniel J. Schulze, Melissa Gooch |
| Institutions | University of Illinois Urbana-Champaign, Intellectual Ventures (United States) |
| Citations | 6 |
Abstract
Section titled “Abstract”In light of breakthroughs in superconductivity under high pressure, and considering that record critical temperatures (T c s) across various systems have been achieved under high pressure, the primary challenge for higher T c should no longer solely be to increase T c under extreme conditions but also to reduce, or ideally eliminate, the need for applied pressure in retaining pressure-induced or -enhanced superconductivity. The topological semiconductor Bi 0.5 Sb 1.5 Te 3 (BST) was chosen to demonstrate our approach to addressing this challenge and exploring its intriguing physics. Under pressures up to ~50 GPa, three superconducting phases (BST-I, -II, and -III) were observed. A superconducting phase in BST-I appears at ~4 GPa, without a structural transition, suggesting the possible topological nature of this phase. Using the pressure-quench protocol (PQP) recently developed by us, we successfully retained this pressure-induced phase at ambient pressure and revealed the bulk nature of the state. Significantly, this demonstrates recovery of a pressure-quenched sample from a diamond anvil cell at room temperature with the pressure-induced phase retained at ambient pressure. Other superconducting phases were retained in BST-II and -III at ambient pressure and subjected to thermal and temporal stability testing. Superconductivity was also found in BST with T c up to 10.2 K, the record for this compound series. While PQP maintains superconducting phases in BST at ambient pressure, both depressurization and PQP enhance its T c , possibly due to microstructures formed during these processes, offering an added avenue to raise T c . These findings are supported by our density-functional theory calculations.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 1960 - Anomalies of electron characteristics in the high pressure region