Skip to content

Broadband Light Extraction from Near-Surface NV Centers Using Crystalline-Silicon Antennas

MetadataDetails
Publication Date2025-03-17
JournalNano Letters
AuthorsMinjeong Kim, Maryam Zahedian, Wenxin Wu, Alex Chengyu Fang, Zhaoning Yu
InstitutionsUniversity of Wisconsin–Madison, Argonne National Laboratory

We use crystalline silicon (Si) antennas to efficiently extract broadband single-photon fluorescence from shallow nitrogen-vacancy (NV) centers in diamond into free space. Our design features relatively easy-to-pattern high-index Si resonators on the diamond surface to boost photon extraction by overcoming total internal reflection and Fresnel reflection at the diamond-air interface and providing modest Purcell enhancement, without etching or otherwise damaging the diamond surface. In simulations, ∼17 times more single photons are collected from a single NV center compared to the case without the antenna; in experiments, we observe an enhancement of ∼9 times, limited by spatial alignment between the NV and the antenna. Our approach can be readily applied to other color centers in diamond, and more generally to the extraction of light from quantum emitters in wide-bandgap materials.