Q-BiC - A Biocompatible Integrated Chip for in vitro and in vivo Spin-Based Quantum Sensing

MetadataDetails
Publication Date2025-03-18
JournalPRX Life
AuthorsLouise Shanahan, Sophia Belser, Jack Hart, Qiushi Gu, Julien R. E. Roth
InstitutionsUniversity of Cambridge
Citations2

Optically addressable spin-based quantum sensors enable nanoscale measurements of temperature, magnetic field, pH, and other physical properties of a system. Advancing the sensors beyond proof-of-principle demonstrations in living cells and multicellular organisms toward reliable, damage-free quantum sensing poses three distinct technical challenges. First, spin-based quantum sensing requires optical accessibility and microwave delivery. Second, any microelectronics must be biocompatible and designed for imaging living specimens. Third, efficient microwave delivery and temperature control are essential to reduce unwanted heating and to maintain an optimal biological environment. Here, we present the quantum biosensing chip (Q-BiC), which facilitates microfluidic-compatible microwave delivery and includes on-chip temperature control. We demonstrate the use of Q-BiC in conjunction with nanodiamonds containing nitrogen vacancy centers to perform optically detected magnetic resonance in living systems. We quantify the biocompatibility of microwave excitation required for optically detected magnetic resonance both in HeLa cells and in the nematode for temperature measurements and determine the microwave-exposure range allowed before detrimental effects are observed. In addition, we show that nanoscale quantum thermometry can be performed in immobilized but nonanaesthetized adult nematodes with minimal stress. These results enable the use of spin-based quantum sensors without damaging the biological system under study, facilitating the investigation of the local thermodynamic and viscoelastic properties of intracellular processes.