Skip to content

Greener Catalytic Oxidation of Azole Fungicides - Coupling EO–O3 on BDD with Kinetics and Mineralization Targets

MetadataDetails
Publication Date2025-12-03
JournalCatalysts
AuthorsJoaquín R. Dominguez, T. González, David Simón-García
InstitutionsUniversidad de Extremadura
AnalysisFull AI Review Included
  • Objective: Decouple and optimize the coupled electro-oxidation (EO) and ozonation (O3) process for degrading a four-azole fungicide mixture (prochloraz, tebuconazole, tetraconazole, penconazole).
  • Anode Material: Boron-Doped Diamond (BDD) — 5 cm × 8 cm flat plate, 40 cm2 active area, paired with an AISI 304 stainless-steel cathode at a 25 mm inter-electrode gap.
  • Statistical Framework: Central Composite Design (CCD) with three coded factors (A = current, B = electrolyte, C = ozone) modeling three responses: abatement (%), pseudo-first-order rate constant k (min−1), and TOC removal (%).
  • Dominant Drivers: Gas-phase O3 concentration is the strongest positive lever for abatement and kinetics; current exhibits curvature-limited diminishing returns (negative A2 term).
  • Inhibitory Effect: Na2SO4 electrolyte has a statistically significant negative effect on TOC removal due to •OH scavenging by SO42−.
  • Optimum Operating Window: Current ≈ 115-135 mA, electrolyte ≈ 1-3 mM, O3 ≈ 7-8 ppm — balancing 33.78% TOC removal with SEC of 1.825 kWh·m−3.
  • Process Verdict: EO-O3 is best positioned as a pre-oxidation or polishing step to enhance biodegradability, not as a stand-alone total mineralization technology.
ParameterValueUnitContext
BDD Anode Dimensions5 × 8cmFlat-plate electrode, 40 cm2 active area
Inter-Electrode Gap25mmBDD anode to AISI 304 SS cathode
Working Volume0.40LJacketed glass batch reactor
Operating Temperature20.0 ± 0.5°CThermostated reactor
Initial pH6.1—Natural pH (no adjustment)
Target Concentration (each azole)5ppm20 ppm total mixed azole load
Current Range (CCD)101 ± 60 (≈ 0-161)mAGalvanostatic mode
Electrolyte Range (Na2SO4)13 ± 7.14 (≈ 1-25)mMSupporting electrolyte
Gas-Phase O3 Range5.5 ± 2.7 (≈ 1-10)ppmInlet ozone dosage
O2/O3 Flow Rate20L·h−1Through porous diffuser
O3 Utilization Efficiency90-95%Optimized EO-O3 conditions
Kinetic Window10minPseudo-first-order regime
Mineralization Window60minTOC plateau region
Abatement R²0.855—Quadratic model fit
k (kinetic) R²0.857—Quadratic model fit
TOC Removal R²0.836—Quadratic model fit
Optimum Current116mAConstrained optimum
Optimum Electrolyte0.992mMNear conductivity threshold
Optimum O37.09ppmGas-phase concentration
Max TOC Removal (Optimum)33.78%At 60 min reaction time
EO Power Density7.20W·L−1Galvanostatic input
O3 Power Density3.75W·L−1Ozonator input
Total Power Density10.95W·L−1Combined system input
Specific Energy Consumption (SEC)1.825kWh·m−3At 10 min, total abatement
EE/O (Electrical Energy per Order)10.19kWh·m−3·order−1Pseudo-first-order metric
Reference Cell Voltage≈ 24VAt I = 0.30 A reference test
HPLC ColumnKinetex C18, 5 µm, 150 × 4.6mmAgilent 1260 Infinity II DAD
  • Reactor Setup: Jacketed glass batch reactor (0.40 L) with porous-diffuser gas inlet, thermostated at 20.0 ± 0.5 °C, natural pH 6.1.
  • Ozone Generation: Sander GmbH 300.1 Labor-Ozonisator fed with O2; gas stream ≈ 1-10 mg·L−1 O3 at 20 L·h−1; off-gas quenched in 2% KI trap.
  • Electrochemical Cell: Two flat-plate electrodes (BDD anode + AISI 304 SS cathode), 5 cm × 8 cm geometry, 25 mm gap, 40 cm2 area; driven by Tektronix PWS2326 power supply in galvanostatic mode.
  • Experimental Design: Central Composite Design (CCD) with 20 runs — 6 axial, 8 factorial, 6 center points; coded factors A (current), B (electrolyte), C (ozone).
  • Operating Envelope: Current 0-161 mA, Na2SO4 1-25 mM, O3 1-10 ppm; center point at 101 mA, 13 mM, 5.5 ppm.
  • Sampling Protocol: 10 min for kinetic/abatement data (pseudo-first-order window); 60 min for TOC mineralization (plateau region).
  • Analytics: HPLC-DAD (Agilent 1260 Infinity II) with Kinetex C18 column (5 µm, 150 × 4.6 mm), acetonitrile / 25 mM H3PO4 mobile phase at 1.0 mL·min−1.
  • Model Fitting: Quadratic response-surface models (linear + 2-factor interactions + quadratic terms) estimated by OLS; adequacy validated via ANOVA F-test, R², adjusted R², and residual diagnostics.
  • Energy Assessment: SEC and EE/O computed from power density × treatment time, with separate accounting for EO and O3 contributions.
  • Applicable Materials:

    • Heavy Boron-Doped PCD anode — the BDD thin-film-on-silicon or BDD-on-niobium variants produced via MPCVD replicate the high oxygen-evolution overpotential and non-adsorbed •OH generation exploited in this study.
    • For research requiring single-crystal electrode baselines, Optical Grade SCD wafers can be doped to BDD-equivalent levels upon request.
    • For scaled-up flow cells beyond 40 cm2, PCD plates up to 125 mm diameter with tunable boron loading (1019-1021 cm−3) provide the rugged, fouling-resistant anode surface this paper identifies as critical for sustained operation.
  • Customization Potential:

    • The 5 cm × 8 cm BDD plate used here is well within 6CCVD’s laser-cutting and custom-dimension service window — substrates can be diced to any rectangular or circular geometry with edge quality suitable for gasket sealing.
    • The AISI 304 cathode can be supplied as Ti, W, or Cu metalized PCD backing plates for bipolar or membrane-electrode-assembly configurations.
    • For hybrid EO-O3 reactor integration, 6CCVD offers internal metalization (Ti/Pt/Au or Ti/W) on the BDD backside for low-resistance current collection and direct busbar soldering.
  • Engineering Support:

    • 6CCVD’s in-house PhD team can assist with material selection for electrochemical advanced oxidation (EAOP) reactor development, including guidance on boron-doping concentration, sp2/sp3 ratio optimization, and surface Ra (< 5 nm achievable on inch-size PCD) for reproducible •OH surface kinetics.
    • For researchers extending this work to higher current densities or pulsed-current protocols, our team can advise on thermal management of the diamond anode — diamond’s exceptional thermal conductivity (≈ 2000 W·m−1·K−1) mitigates the curvature-limited plateaus observed in the A2 term.
    • We can also support custom free-standing SCD or PCD windows for in-situ Raman/FTIR monitoring of •OH and O3 speciation during EO-O3 operation.
  • Call to Action:

    • For custom specifications, boron-doping consultation, or metalization design for EAOP research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract

This study evaluates the abatement of four common azole fungicides—prochloraz, tebuconazole, tetraconazole, and penconazole—using ozonation (O3), electro-oxidation (EO on boron-doped diamond anode), and their coupling (EO-O3). A central composite design (CCD) with three coded factors—current (A), electrolyte (B), and ozone concentration in the gas phase (C)—was employed to model three responses: pollutant abatement (%), apparent pseudo-first-order rate constant k (min−1), and TOC removal (%). Quadratic models showed good in-samples (R2 ≈ 0.84-0.86). Ozone and current dominate abatement and kinetics (with curvature in current), while the electrolyte penalizes mineralization and narrows the window for TOC removal. Under optimal conditions, 116 mA (current), 0.992 mM (electrolyte), and 7.09 ppm (ozone concentration), the EO-O3 configuration results in a TOC removal of 33.78%. At a reaction time of 10 min (total abatement of the pollutants), the hybrid EO-O3 configuration exhibits a specific energy consumption (SEC) of 1.825 kWh·m−3. We compare trends with the last decade of literature on ozone-based EAOPs, electro-peroxone variants, and BDD anodic oxidation, and outline practical guidance for its application and scale-up, and model refinement in predictive settings.

  1. 2021 - Azole and strobilurin fungicides in source, treated, and tap water from wuhan, Central China: Assessment of human exposure potential [Crossref]
  2. 2023 - Comparative insight of pesticide transformations between river and wetland systems [Crossref]
  3. 2022 - Effect of electrolyte composition on electrochemical oxidation: Active sulfate formation, benzotriazole degradation, and chlorinated by-products distribution [Crossref]
  4. 1983 - Rate constants of reactions of ozone with organic and inorganic compounds in water—I: Non-dissociating organic compounds [Crossref]
  5. 2024 - The Role of Ozonation as an Advanced Oxidation Process for Attenuation of 1, 4-Dioxane in Potable Reuse Applications [Crossref]
  6. 2022 - Ozonation for remediation of pesticide-contaminated soils at field scale [Crossref]
  7. 2025 - Micro and nanobubbles enhanced ozonation technology: A synergistic approach for pesticides removal [Crossref]
  8. 2025 - Research Progress of Micro-Nano Bubbles in Environmental Remediation: Mechanisms, preparation methods, and applications [Crossref]