Skip to content

Particle Size of 45S5 Bioactive Glass Affected the Enamel Remineralization

MetadataDetails
Publication Date2015-03-01
JournalMaterials science forum
AuthorsZhi Hong Dong, Chang Chun Zhou
InstitutionsChengdu University, Sichuan University
Citations2

In order to repair the etched human dental enamel, 45S5 bioactive glass with different particle size was used to remineralization enamel in vitro. 45S5 bioactive glass powder was sieved, and divided into the three groups. Freshly sound human second molar teeth from patients were extracted and specimens of dentine-enamel junction were prepared under water-cooled diamond saw, then the enamel surface was polished and finally rinsed. The enamel samples were soaked in simulated oral fluid (SOF) for 5 days. Particle size distribution, topological images and mechanical properties such as hardness and reduced modulus of enamel surface were evaluated by the laser particle size analyzer, atomic force microscope (AFM) and nanoindentation technology. The results indicated that the adhered particle size onto the enamel surface was concentrated on the 1-10 μm. With the decreasing particle size, adhesive capacity onto the enamel surface increased, but the mechanical properties decreased gradually after soaking in SOF for 5 days. In a short period time, Group 2 particles are suitable of repair the etched enamel, and further improve its mechanical properties. This study suggests that proper size 45S5 bioactive glass may be used to repair the acid etched teeth as a toothpaste additive.