Design and fabrication of an elliptical micro-lens array with grating for laser safety
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-10-15 |
| Journal | Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE |
| Authors | L. H. Li, Boqi Wu, C. Y. Chan, Wing Bun Lee, L. Dong |
| Institutions | Changchun University of Science and Technology, Hong Kong Polytechnic University |
Abstract
Section titled āAbstractāWith the enormous expansion of laser usage in medicine, industry and research, all facilities must formulate and adhere to specific safety methods that appropriately address user protection. The protective ellipticalal microstructure with grating is a novel technology which can provide the principal means of ensuring against ocular injury, and must be worn at all times during laser operation. On the basis of Fresnelās law and the diffractive law, Solidworks and Lighttools software are applied to design the elliptical micro-lens array and correspondent grating. The height of the microstructure is 100um and its period is 3mm. The period of grating is 5um. It is shown that the amount of emergent light of a specific wavelength (1064nm) can reflect more than 40° from the incident light through simulation, while the incident light is perpendicular to the microstructure. The fabrication adopts the ultra-precision single point diamond method and injection molding method. However, it is found in the test that the surface roughness has a serious effect on the angle between the emergent and incident light. As a result, the element can reflect the vertical incidence beam into a tilted emergent beam with a certain angular degree, as well as protecting users from laser damage injures.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2014 - Eye and Face Protection Manual[J]
- 2005 - Application and protection of laser technology [J][J]