Recombination centers in 4H-SiC investigated by electrically detected magnetic resonance and ab initio modeling
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-05-05 |
| Journal | Journal of Applied Physics |
| Authors | Jonathon Cottom, G. Gruber, P. Hadley, Markus Koch, Gregor Pobegen |
| Institutions | Infineon Technologies (Austria), Siemens (Austria) |
| Citations | 16 |
Abstract
Section titled āAbstractāElectrically detected magnetic resonance (EDMR) is a powerful technique for the observation and categorization of paramagnetic defects within semiconductors. The interpretation of the recorded EDMR spectra has long proved to be challenging. Here, defect spectra are identified by comparing EDMR measurements with extensive ab initio calculations. The defect identification is based upon the defect symmetry and the form of the hyperfine (HF) structure. A full description is given of how an accurate spectrum can be generated from the theoretical data by considering some thousand individual HF contributions out of some billion possibilities. This approach is illustrated with a defect observed in nitrogen implanted silicon carbide (SiC). Nitrogen implantation is a high energy process that gives rise to a high defect concentration. The majority of these defects are removed during the dopant activation anneal, shifting the interstitial nitrogen to the desired substitutional lattice sites, where they act as shallow donors. EDMR shows that a deep-level defect persists after the dopant activation anneal. This defect is characterized as having a gcā„B=2.0054(4) and gcā„B=2.0006(4), with pronounced hyperfine shoulder peaks with a 13 G peak to peak separation. The nitrogen at a carbon site next to a silicon vacancy (NCVSi) center is identified as the persistent deep-level defect responsible for the observed EDMR signal and the associated dopant deactivation.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2004 - Silicon Carbide: Recent Major Advances
- 2011 - Silicon Carbide: Volume 1