Real-Time Charge Control of Diamond Quantum Sensors
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Journal | OSA Quantum 2.0 Conference |
| Authors | David A. Hopper, J. Lauigan, TzuāYung Huang, Lee C. Bassett |
| Institutions | University of Pennsylvania |
Abstract
Section titled āAbstractāWe use real-time feedback to deterministically initialize a nitrogen-vacancyās charge state at room temperature, and demonstrate improved spin readout efficiency resulting in a factor-of-20 speedup for a typical quantum sensing experiment.