Toward Accurate Diamond Quantum Sensing
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2023-01-01 |
| Journal | JPS Hot Topics |
| Authors |
Abstract
Section titled āAbstractāA systematic investigation of the optical power dependence of the response of diamond quantum sensors provides valuable guidelines for accurate magnetic field measurements.