Exploration of a high-precision measurement scheme for current sensors based on diamond NV color centers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-05-01 |
| Journal | Journal of Physics Conference Series |
| Authors | Long Zhao, Xin Wang, Rujia Qiu, Dongbo Song, Teng Tian |
| Citations | 1 |
Abstract
Section titled āAbstractāAbstract A high-precision measurement scheme for current sensors based on diamond NV color centers was verified. In the research process, diamond crystals containing a large number of NV color centers are applied as the probe of the sensor, and the magnetic field generated by the current is measured to explore the relationship between the current intensity and the fluorescence intensity of the NV color centers and the polarization resonance, to carry out simulation experiments, and finally to obtain the results of the effect of the concentration of the NV color centers on the performance of the sensor. The results of simulation experiments show that the accuracy of the current measurement is within 100-500 A, and the result is 0.3%. By applying NV color centers to current measurement, good results have been obtained in terms of accuracy and frequency response range, enabling high-precision current measurement as well as providing monitoring and analysis of high-frequency current inrush.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2023 - Spin measurement and modulation of 14 N nuclei within diamond NV color-centered system
- 2023 - Weak magnetic field measurement based on diamond NV color centers
- 2022 - Optical and Spin Properties of NV Center Ensembles in Diamond Nano-Pillars [Crossref]
- 2023 - Fiber optic quantum sensing based on diamond nitrogen-vacancy color centers
- 2023 - Enhanced fluorescence of NV color centers based on localized surface equipartition excitations Ag/diamond nanostructures
- 2021 - Hyperfine Interactions in the NV-13C Quantum Registers in Diamond Grown from the Azaadamantane Seed [Crossref]
- 2023 - Sensitivity analysis of continuous temperature measurement of diamond nitrogen-vacancy color centers
- 2023 - Clustered diamond NV color-centered quantum spin-directed excitation method for magnetic sensing enhancement
- 2022 - Application of diamond NV color-core current transformer