Generation of Nitrogen-Vacancy Center Pairs in Bulk Diamond by Molecular Nitrogen Implantation

MetadataDetails
Publication Date2016-02-01
JournalChinese Physics Letters
AuthorsZhao-Jun Gong, Xiang-Dong Chen, Li Congcong, Shen Li, Bowen Zhao
InstitutionsCAS Key Laboratory of Urban Pollutant Conversion, University of Science and Technology of China
Citations2

The coupled negatively charged nitrogen-vacancy (NVāˆ’) center system is a promising candidate for scalable quantum information techniques. In this work, ionized nitrogen molecules are implanted into bulk diamond to generate coupled NVāˆ’ center pairs. The two-photon autocorrelation measurement and optically detected magnetic resonance measurement are carried out to confirm the production of the NVāˆ’ center pair. Also, both 1.3 μs decoherence time and 4.9 kHz magnetic coupling strength of the NVāˆ’ center pair are measured by controlling and detecting the spin states. Along with nanoscale manipulation and detection methods, such coupled NVāˆ’ centers through short distance dipole-dipole interaction would show high potential in scalable quantum information processes.